BS EN ISO 07046 — Countersunk Flat Head Screws (Type H or Type Z Cross Recess, Product Grade A) Series

Common Head Style with Type H or Type Z Cross Recess, Product Grade A (ISO 7046)

🔩 BS EN ISO 7046 specifies the dimensions, materials, property classes and test requirements for countersunk flat head screws with a cross recess — among the most widely used fastener product standards in mechanical assembly, instruments, electrical/electronic equipment and woodworking. In the UK the series is implemented under Technical Committee FME/9/3, “Fasteners — Product Standards”, as the official British adoption of ISO 7046 and EN ISO 7046, classified under ICS 21.060.10. The series has two parts, addressing screws of different materials and property classes.

💡 Cross-recess screws are the “most universal” fasteners: the H (Phillips) and Z (Pozidriv) recesses circulate globally, so any manufacturer’s products made to ISO 7046 are interchangeable.

1. Scope and General Framework 📌

The series applies to product grade A countersunk flat head screws — the grade with the tightest dimensional tolerances and highest precision, suited to applications demanding assembly accuracy. The head is countersunk (flat), with its top surface flush with the joined part, used mainly where a flat, protrusion-free surface is required.

  • BS EN ISO 7046-1:2011: specifies steel screws of property class 4.8 (type H or Z cross recess).
  • BS EN ISO 7046-2:2011: specifies steel screws of property class 8.8, stainless steel screws and non-ferrous metal screws (type H or Z cross recess).

Both parts give the nominal size range, head dimensions, thread specifications, cross-recess dimensions, materials and performance requirements, together with the corresponding test methods and marking rules.

⚠️ The difference between product grade A and ordinary grades (B, C) is dimensional tolerance: grade A screws have tighter head, shank and thread tolerances for precision assembly; for low-precision general use, a lower product grade may be selected to reduce cost.

2. Series Structure and Technical Highlights 🔢

StandardTitleMaterial / property classTypical application
BS EN ISO 7046-1:2011Countersunk flat head screws (common head style) with type H or type Z cross recess — Product grade A — Part 1: Steel of property class 4.8Carbon steel, class 4.8General machinery, electrical, furniture assembly
BS EN ISO 7046-2:2011Part 2: Steel screws of property class 8.8, stainless steel screws and non-ferrous metal screwsCarbon steel 8.8, stainless steel, non-ferrous metalsHigher strength, corrosion resistance and special duties

Part 1 focuses on medium/low-strength carbon steel screws (class 4.8) for general loading and ordinary environments; Part 2 covers high-strength carbon steel (8.8), stainless steel (e.g. A2, A4) and non-ferrous metals (e.g. brass, aluminium) for high strength, corrosion resistance, or special electrical/magnetic/conductive requirements.

3. Dimensions and Tolerances 📐

The standard specifies key dimensions and tolerances, including:

  • Thread specification and size: nominal diameter, pitch, thread length and the nominal length series.
  • Head dimensions: countersunk head diameter, head height, countersink angle (typically 90°) and head fillet.
  • Cross-recess dimensions: recess width, depth, bottom shape and size code for type H or Z.
  • Product grade A tolerances: limit deviations of head, shank and thread, ensuring assembly interchangeability and accuracy.
✅ The key to a countersunk screw is the fit between the head and the countersink: head angle, diameter and countersink size must match, or the head will sit too low or protrude, or even fracture during tightening. Check the countersink dimensions per the standard during assembly design.

4. Materials and Property Classes 🔧

The standard specifies screws by property class and material:

  • Property class 4.8 (carbon steel): nominal tensile strength about 400 MPa, yield ratio about 0.8, for general structural joints.
  • Property class 8.8 (carbon steel): nominal tensile strength about 800 MPa, yield ratio about 0.8, for higher-strength joints.
  • Stainless steel: specified by material group (e.g. austenitic A2, A4), with good corrosion resistance for wet, outdoor and food/pharmaceutical environments.
  • Non-ferrous metals: brass, aluminium and alloys, for electrical, decorative and non-magnetic needs.
🚨 Property class and material directly determine load capacity and corrosion resistance — never select on appearance alone. High-strength 8.8 screws without coating in wet environments risk hydrogen embrittlement and stress corrosion; in high-chloride environments use a high-molybdenum grade (e.g. A4).

5. Testing and Marking Rules 📋

The standard specifies the relevant mechanical tests (e.g. tensile, hardness, torque) and surface-treatment requirements, plus the marking rules:

  • Product marking: standard number, thread specification, nominal length, property class (or material group), surface treatment and manufacturer’s identification.
  • Test methods: per companion standards such as ISO 898 (mechanical properties of fasteners), checking hardness, tensile, torque and surface condition.
  • Surface treatment: zinc plating, nickel plating, dacromet etc., for corrosion protection and to influence assembly friction coefficient and preload.

6. Frequently Asked Questions ❓

❓ Q: Can type H and type Z recesses be used interchangeably?
A: No. H (Phillips) and Z (Pozidriv) have different recess forms and require different driver tips; mixing them causes the driver to slip and damages the screw head.
❓ Q: How do I choose between class 4.8 and 8.8 screws?
A: By the load and strength requirement of the joint. Use 4.8 for non-load-bearing or light-duty connections; use 8.8 where higher preload and greater load are required, matching the nut and washer classes.
❓ Q: Why are countersunk screws so demanding on the countersink?
A: The screw relies on the conical head face seating in the countersink to carry the tightening torque and shear load; if the countersink is wrong, the head protrudes, loosens or loads unevenly, and may even fracture.
❓ Q: Why do stainless steel screws sometimes seize?
A: Stainless steel is prone to cold welding and galling, especially with tight thread fits or at elevated temperature. Use a molybdenum grade, apply an anti-seize coating, or use a suitable tolerance fit.
❓ Q: What is the size range of these screws?
A: The standard defines size series by thread specification, typically covering small countersunk screws from about M1.6 to M10; the exact range is given in the dimensional tables of the standard text.
🔒