BS EN ISO 06603 — Plastics — Determination of Puncture Impact Behaviour of Rigid Plastics (Non-Instrumented and Instrumented Impact Testing)

Part 1: Non-Instrumented Impact Testing and Part 2: Instrumented Puncture Testing (ISO 6603)

🧪 BS EN ISO 6603 specifies methods for determining the behaviour of rigid plastics under falling-weight (puncture) impact, and is an important means of evaluating impact toughness and of distinguishing brittle from ductile fracture. In the UK the series is implemented under Technical Committee PRI/21, “Testing of plastics”, as the official British adoption of ISO 6603 and EN ISO 6603, classified under ICS 83.080.01. The series consists of two parts: Part 1 specifies the non-instrumented impact test, which records only whether failure occurs and the energy absorbed; Part 2 specifies the instrumented puncture test, which simultaneously records the force—displacement—time history and yields a full set of fracture parameters.

⚠️ The source material for Part 1 (BS EN ISO 6603-1:2000) in this series is a scanned copy and the full text could not be read. This article is written from public domain knowledge of the standard (test principle, specimens and impact conditions, result evaluation) and expands the instrumented method (BS EN ISO 6603-2:2000) from the readable text. Always cite the official BSI publication.

1. Scope and General Framework 📌

The series applies to rigid plastics — materials with a relatively high modulus under the specified conditions that do not deform appreciably in a plastic manner, such as polystyrene (PS), polycarbonate (PC), poly(methyl methacrylate) (PMMA), rigid poly(vinyl chloride) (PVC) and reinforced plastic sheet. The test simulates a point (puncture) impact such as a falling object striking a panel or enclosure during service or transport.

  • BS EN ISO 6603-1:2000 (non-instrumented): a falling dart strikes the specimen; by using darts of different mass or different drop heights, the energy required to cause failure is determined and expressed as “impact energy” or “critical impact energy”.
  • BS EN ISO 6603-2:2000 (instrumented): during the impact the force is recorded synchronously by a sensor, yielding force—time and force—displacement curves from which peak force, failure energy and total impact energy are calculated, together with an assessment of fracture mode.

Both parts use plate specimens, typically square (e.g. 60 mm × 60 mm) or circular, with thickness produced to specification. The striker has a spherical or hemispherical end and impacts the centre of the specimen by free fall or mechanical drive.

2. Series Structure and Technical Highlights 🔢

StandardTitleTest typeKey output parameters
BS EN ISO 6603-1:2000Determination of puncture impact behaviour of rigid plastics — Part 1: Non-instrumented impact testingNon-instrumented falling-weight impactImpact energy, critical impact energy, brittle/ductile classification
BS EN ISO 6603-2:2000Part 2: Instrumented puncture testingInstrumented falling-weight impactPeak force, failure energy, total impact energy, force—time/displacement curves, fracture mode

The non-instrumented method (Part 1) is simple and low-cost, suited to routine quality control; the instrumented method (Part 2) is information-rich, resolving how the material absorbs energy during the impact, and suits materials development, failure analysis and quality grading.

💡 The two methods are complementary rather than alternatives: use Part 1 for fast, high-throughput screening; use Part 2 to understand fracture mechanics and quantify the ductile-to-brittle transition. Many polymer laboratories run both.

3. Test Principle and Key Conditions 🎯

The test centres on striking the specimen with a striker of defined mass and shape at a defined velocity, and measuring the material response during or after the impact. Key conditions include:

  • Conditioning: plastics are sensitive to temperature and humidity; specimens should be conditioned per ISO 291 at standard laboratory conditions (e.g. 23 °C / 50 % RH) and tested within a specified time.
  • Impact velocity: the velocity of the free-falling dart is set by drop height; testing is typically at about 2–4 m/s, corresponding to the specified height.
  • Striker mass and geometry: a spherical face of specified diameter; impact energy is varied by changing striker mass (or added weights).
  • Specimen thickness: impact behaviour is thickness-sensitive; results must state the thickness, and energies from different thicknesses should not be compared directly.
🚨 Impact tests are highly sensitive to operator factors: loose clamping, a worn striker, an impact point off the specimen centre, and residual stress or machining defects in the specimen can all change the fracture energy and mode, even reversing a “brittle” and “ductile” conclusion. Always calibrate, inspect the striker and clamp correctly before testing.

4. Data Evaluation in the Instrumented Test 📊

In Part 2 a force transducer on the striker or support records the force—time signal at a very high sampling rate. From this the following are derived:

  • Peak force (Fp): the maximum impact force during the event, reflecting the material’s greatest resistance to the impact load.
  • Failure energy (Ef): the energy absorbed from the start of impact to failure (sudden drop in force), obtained by integrating the force—displacement curve.
  • Total impact energy (Et): the total energy absorbed during the whole event, including continued penetration after failure.
  • Fracture mode: from the shape of the force—displacement curve and the maximum displacement, brittle fracture (low energy absorption, rapid fall after peak), ductile fracture (large absorption, gentle curve) and puncture can be distinguished.
✅ The most valuable contribution of instrumented data is the “energy absorption history”: two materials may have similar failure energies but very different force—displacement shapes, which directly determines how the product fails in a real impact — a key input for material selection and structural design.

5. Engineering Practice 🛠️

  • 🔍 Quality control of plastic sheet and film: puncture impact is a common type-test and release-test item for packaging, construction and automotive interior panels.
  • 📊 Materials development and modification: instrumented impact curves reveal the effect of toughening modifiers and whether a plastic deformation zone is formed.
  • 📋 Ductile-brittle transition studies: a series of impact tests at different temperatures yields the transition temperature, guiding low-temperature material selection.
  • 🔧 Failure analysis: impact testing of fractured products, combined with fracture-surface morphology, distinguishes impact from fatigue failure.

6. Frequently Asked Questions ❓

❓ Q: What is the difference between ISO 6603 and ISO 179 (Charpy)?
A: ISO 6603 is a falling-weight puncture impact on a plate with a point load; ISO 179 is a pendulum bending impact on a small notched or unnotched bar. They simulate different situations and are not interchangeable.
❓ Q: Why is conditioning essential?
A: The impact performance of plastics is highly sensitive to temperature and moisture content. Without conditioning the same batch can give very different results in different seasons, making comparison impossible.
❓ Q: Can Part 1 and Part 2 results be compared directly?
A: Not simply. Specimen, striker and impact conditions are broadly the same, but the definition of failure energy in Part 2 differs slightly from the “impact energy” of Part 1. Always state the standard used in the report.
❓ Q: Does specimen thickness matter much?
A: Very much. Thin specimens tend to puncture, thick ones to crack or delaminate, and both energy and mode may change. Always report the thickness and be cautious comparing across thicknesses.
❓ Q: Is the series limited to a single plastic?
A: No. It applies to various rigid plastics and some plastic composite sheet, provided the material behaves rigidly under the test conditions.
🔒