🎨 BS EN ISO 2884 specifies methods for determining the viscosity of paints and varnishes using rotary viscometers. Viscosity is one of the most important rheological properties of coatings, directly affecting application performance (brush, roller, spray), levelling and sagging behaviour, storage stability and film quality. The series comprises Part 1 (cone-and-plate viscometer at a high rate of shear) and Part 2 (disc or ball viscometer at a specified speed), covering high and medium-to-low shear rate ranges respectively, and is widely used for quality control of paints, inks and similar liquid coating materials.
The BS EN ISO 2884 series consists of two parts distinguished by shear-rate range and viscometer type:
| Part | Standard Title | Measurement Conditions | Primary Application |
|---|---|---|---|
| BS EN ISO 2884-1 | Paints and varnishes — Determination of viscosity using rotary viscometers — Part 1: Cone-and-plate viscometer operated at a high rate of shear (2006, from ISO 2884-1:1999, aligned with BS 3900-A7-1) | High rate of shear, cone-and-plate | Simulating spraying, high-speed application shear |
| BS EN ISO 2884-2 | Paints and varnishes — Determination of viscosity using rotary viscometers — Part 2: Disc or ball viscometer operated at a specified speed (2006, from ISO 2884-2:2003, aligned with BS 3900-A7-2) | Specified speed, disc or ball | Routine coating viscosity control, medium-to-low shear |
Basic principle: A rotary viscometer measures the resisting torque (or the torque required to maintain a specified speed) of a geometry (cone, disc, ball, etc.) immersed in the liquid, and calculates viscosity using the instrument constant. The higher the viscosity, the greater the torque at a given speed.
Shear-rate control: The cone-and-plate viscometer creates a uniform shear field in the small gap between the cone and plate, allowing measurement at very high shear rates; the disc/ball viscometer measures at a specified speed, giving lower or undefined shear rates, providing mainly relative/conditional viscosity.
| Element | Description |
|---|---|
| Sample preparation | Coatings should be uniform, free of bubbles, filtered if necessary; sample as specified and control temperature |
| Temperature control | Viscosity is temperature-sensitive; measure at the specified temperature with accurate control |
| Measurement geometry | Cone, disc or ball, selected per standard and viscosity range |
| Speed/shear rate | Part 1: high shear rate; Part 2: specified speed |
| Result reading | Read torque or viscosity; convert to dynamic viscosity (mPa·s) if necessary |
Part 1 — High shear rate cone-and-plate: The cone-and-plate viscometer provides a uniform shear field, requires only a small sample and reaches steady state quickly, making it suitable for simulating spraying and high-speed coating application. Results at high shear rate reflect the flow resistance of the coating under high shear, closely related to application behaviour.
Part 2 — Specified-speed disc/ball: A disc or ball viscometer operates at a specified speed, is simple to operate and gives good repeatability, making it suitable for routine production control. Values obtained are conditional; results vary with speed, geometry and temperature.
| Method | Shear Level | Features | Typical Application |
|---|---|---|---|
| Cone-and-plate (Part 1) | High shear rate | Uniform shear field, small sample, fast | Spraying, high-speed application rheology |
| Disc/ball (Part 2) | Specified speed (medium-low shear) | Simple, good repeatability | Production control, routine viscosity check |