BS EN ISO 02812 — Paints and Varnishes Determination of Resistance to Liquids Standard Series (ISO 2812)

Paints and Varnishes — Determination of Resistance to Liquids(ISO 2812)

🎨 BS EN ISO 2812 (series number BS EN ISO 02812) is the series by which BSI adopts the European standard EN ISO 2812, itself identical to the ISO 2812 series, prepared with UK participation through BSI Committee STI/10 (Test methods for paints). The series specifies the determination of the resistance of paint and varnish coatings to liquids, test standards used to evaluate a film’s ability to resist attack and appearance change when exposed to water, solvents, acids/alkalis, cleaners, and oils. The parts of the series specify immersion methods (non-aqueous liquids, water) and absorption-medium (spot test) methods, and are widely used by the automotive, household-appliance, construction, and industrial-protective-coating industries for formulation development, quality control, and acceptance of chemical-resistance requirements.

💡 “Liquid resistance” is a hard requirement in many applications: kitchen worktops must resist cleaners, automotive interiors must resist sunscreen, and tank linings must resist chemical media — the ISO 2812 series provides unified, reproducible procedures for these evaluations.

1. Series Overview and Scope 📌

The series applies to films of various paints and varnishes after application and drying/curing, and is used to measure their resistance when acted upon by a specific liquid medium. Results are evaluated by observing phenomena such as blistering, loss of gloss, discolouration, softening, loss of adhesion, swelling, or peeling, and grading them per the standard. Each part is numbered “Part x”: Part 1 specifies the immersion method in liquids other than water; Part 2 specifies the water immersion method; Part 3 specifies the absorption-medium method (droplet test) using filter paper or similar; later parts extend these with specific media and conditions.

The series is technically identical to ISO 2812, with the UK version adopting EN ISO 2812 through BSI and superseding earlier scattered UK corresponding methods. In practice, coating suppliers issue media-resistance data per the series, and users select the corresponding part by application medium for acceptance testing.

⚠️ Some parts of this series are scanned document versions; the related sections of this article are written from public domain knowledge. Always refer to the official BSI published version for exact immersion time, temperature, and grading details.

2. Series Structure and Part List 📋

Standard NumberYearSubjectDocument Status
BS EN ISO 2812-12007Immersion in liquids other than waterReadable text
BS EN ISO 2812-22007Water immersion methodReadable text
BS EN ISO 2812-32012Absorption-medium method (spot test)Readable text
BS EN ISO 2812-42007Related spot-test provisions of Part 4Scanned version
BS EN ISO 2812-52007Related test provisions of Part 5Scanned version
✅ Each of the three main methods has its strengths: non-aqueous immersion for chemical-media evaluation, water immersion for water/moisture resistance, and the absorption-medium (spot) method for localised, small-volume liquid contact — method selection should match the real service environment.

3. Key Technical Requirements 🔬

3.1 Immersion in Liquids Other than Water (Part 1)

Part 1 specifies immersion of the coated specimen in liquid media other than water (e.g. solvents, acids, alkalis, oils, cleaners), followed by removal, cleaning, and assessment of film change after the specified temperature and time. It is used to evaluate the coating’s resistance to a specific chemical medium; the medium and immersion conditions (temperature, time) are usually agreed by the product specification.

3.2 Water Immersion Method (Part 2)

Part 2 specifies immersion of the specimen in water (distilled water or specified quality), assessing blistering, loss of gloss, softening, and other changes after the specified temperature (e.g. 23 °C or 40 °C) and time. Water resistance is an important indicator for waterborne coatings and moisture-barrier films and is highly sensitive to cross-link density and adhesion.

3.3 Absorption-Medium Method (Spot Test, Part 3)

Part 3 specifies using an absorption medium (e.g. a filter-paper disc) wetted with the test liquid and held against the coating surface, removing it after the specified time and assessing changes in the contact area. This method suits simulating a single droplet resting on a horizontal surface for a long time (e.g. cup rings on desktops/worktops, chemical splashes); it uses little liquid, defines a clear area, and facilitates localised failure analysis.

⚠️ Result assessment depends heavily on viewing conditions and the rating table: blister density and size, gloss loss, and colour change must all be described per the standard grades. For consistency, have the same operator assess the same batch under uniform lighting and viewing angle.

4. Engineering Practice 🛠️

  • 🚗 Automotive interiors and bodies: evaluate resistance of painted surfaces to sunscreen, car-wash fluids, fuel, and coolant.
  • 🏠 Furniture and worktops: use the spot test to simulate cup rings and discolouration caused by coffee, vinegar, and alcohol.
  • 🏭 Industrial protective coatings: select immersion methods by contact medium to evaluate chemical resistance of tank and pipe interiors.
  • 🔬 Formulation development: screen resins, additives, and curing conditions at the R&D stage to optimise media resistance.
  • 📋 Procurement acceptance: include water- and solvent-resistance indicators in technical agreements and accept incoming coatings or products per the series methods.

5. Frequently Asked Questions ❓

❓ Q: What is the relationship between BS EN ISO 2812 and ISO 2812?
A: BS EN ISO 2812 is the UK adoption of EN ISO 2812, which is identical to ISO 2812. Technical content is the same; the BS version adds a national foreword.
❓ Q: How do the immersion methods (Part 1 vs Part 2) differ in selection?
A: Choose by medium — non-aqueous chemical media (solvents, acids, alkalis, oils) use Part 1; water or moisture (rain, humidity, washing) uses Part 2. Both can be run to cover the requirement.
❓ Q: Are spot-test and immersion results comparable?
A: Not fully. The spot test is localised static contact; immersion is full-surface contact; the stress state and liquid penetration depth differ. Reports must state the method used; typically the same application scenario always uses the same method for comparison.
❓ Q: How is the immersion temperature determined?
A: Temperature sets the test severity. Room temperature (23 °C) is common; higher temperatures (e.g. 40 °C) simulate hot/humid conditions. The exact temperature, time, and water quality are agreed by the product specification or between supplier and user, and must be fully recorded in the report.
🔍 Q: Can scanned parts be cited directly?
A: This article only describes the scanned parts at a high level. Formal testing and citation must be based on the official BSI published version, verifying the exact media, conditions, and grading details in the original text.
🔒