BS EN ISO 1167 — Thermoplastics Pipes Resistance to Internal Pressure Series

Standard Series (Part 1: General Method & Part 2: Preparation of Pipe Test Pieces)

🔧 BS EN ISO 1167 is the BSI-published series adopting the European Standard EN ISO 1167, identical to ISO 1167. It specifies methods for determining the resistance to internal pressure (hydrostatic strength) of thermoplastics pipes, fittings and assemblies, and is the most important long-term performance test in the plastics piping industry. Plastic pipes for water supply, gas, drainage and industrial fluid transport are typically designed for service lives of 50 years or more, so internal-pressure tests are used to derive the “hoop stress versus time” relationship, from which the long-term hydrostatic strength is extrapolated as the basis for pipe rating (e.g. SDR and pressure classes). The series has two parts: Part 1 specifies the general test method, and Part 2 specifies the preparation of pipe test pieces. The series supersedes the former BS EN 921.

💡 BSI Technical Committee PRI/88 (Plastic Pipes) via subcommittee PRI/88/4 (Test Methods) manages UK participation. The series works with ISO 9080 (extrapolation of long-term hydrostatic strength) to form the data chain for pipe life design.

1. Series Overview and Scope 🎯

The basic principle of the internal-pressure test: a pipe specimen with sealed ends is filled with the test medium (usually water) and subjected to a constant internal pressure at a set temperature, and the time to failure (or survival to a specified time) is recorded. Sets of “stress-temperature-time” data from multiple specimens enable the construction of the material’s long-term strength curve. The series is classified under ICS 23.040.45/23.040.20 (plastics pipes and fittings).

StandardTitleMain Content
BS EN ISO 1167-1:2006Thermoplastics pipes, fittings and assemblies for the conveyance of fluids — Resistance to internal pressure — Part 1: General methodTest types, test medium, pressure application, temperature control, end sealing and result judgement
BS EN ISO 1167-2:2006Thermoplastics pipes, fittings and assemblies for the conveyance of fluids — Resistance to internal pressure — Part 2: Preparation of pipe test piecesSpecimen length, end preparation, sealing method and conditioning requirements
⚠️ Temperature control is critical in this test: temperature deviation markedly changes the creep and yield behaviour of plastics and hence the failure time. The test chamber temperature field must be uniform and stable.

2. Part 1: General Method 🧪

BS EN ISO 1167-1:2006 specifies the general test procedure for internal-pressure testing:

  • Test types: distinguishes “failure test” (recording time to rupture) from “durability test” (surviving a set time without failure) and similar types.
  • Apparatus: pressurisation system, thermostatted bath/chamber, specimen sealing fittings and pressure-measurement instrument specifications.
  • Pressure and temperature: rapid pressurisation with stabilisation, temperature tolerance and medium requirements.
  • Result judgement: validity of failure location (failure in the mid-section is valid; seal-end failures warrant retesting) and reporting content.
💡 Failure location is the first validity check: if rupture occurs at the sealing fittings or clamped end zones, the stress state deviates from the hoop-tension assumption — treat that test as invalid and take new specimens.

3. Part 2: Preparation of Pipe Test Pieces 📏

BS EN ISO 1167-2:2006 provides detailed preparation requirements for pipe specimens to ensure representativeness and repeatability:

  • Specimen length: free length determined by pipe outer diameter, so the end-sealing clamping does not affect the central measuring section.
  • End preparation: squareness of end faces, sealing fitting type (taper grips, flanged type) and installation torque.
  • Conditioning: specimens are conditioned under standard conditions (temperature, time), and the assembly state of pipe/fitting combinations is recorded.
  • Dimension measurement: accurate measurement of internal diameter, outer diameter and wall thickness for hoop-stress calculation.
🚨 Over-tight end-sealing clamps cause stress concentration and premature failure in the clamp zone; too loose causes leaks. Clamping parameters must be set per Part 2 and recorded in the report.

4. Key Technical Points 🔍

TopicPart 1 (General Method)Part 2 (Specimen Preparation)
Core contentTest procedure and judgementSpecimen geometry and handling
Pressure controlPressurisation and stabilisation methodNot applicable (test execution)
End conditionsSealing effectivenessClamping and fitting installation
Hoop stressCalculated from dimensions and pressureProvides accurate dimensions
Typical useType testing, acceptanceTest preparation specification

5. Engineering Practice 🛠️

  • Long-term strength extrapolation: use ISO 9080 with multi-temperature, multi-stress data to extrapolate the 50-year long-term hydrostatic strength at 20 °C and determine the pipe MRS rating.
  • Type testing: run internal-pressure type tests on new products under the conditions (temperature, stress, time) required by the product standard.
  • Quality control: sample production batches with short-term (e.g. 1 h, 100 h) internal-pressure tests to monitor process stability.
  • Failure analysis: retest samples from pipes that failed in service; combine fracture morphology to decide whether the cause is material degradation or installation issues.

6. FAQ ❓

❓ Why do plastic pipes need “long-term” internal-pressure tests?
Answer: Plastics are viscoelastic; long-term pressurisation causes creep and slow crack growth. Short-term strength far exceeds long-term strength; only long-term data reliably extrapolate the design life.
❓ Is a failure at the clamps valid?
Answer: No. Stress concentration and constraint at the clamps mean the rupture does not represent the pipe body performance; prepare new specimens and check the clamping process.
❓ How much does temperature affect the results?
Answer: Greatly. Higher temperature accelerates creep and failure significantly; the failure time of the same specimen at high temperature is far shorter than at low temperature, which is why long-term tests run at several temperatures.
❓ How are pipe/fitting assemblies tested?
Answer: Assemble the fitting and pipe per the installation procedure, then perform the internal-pressure test on the assembly to evaluate the overall sealing and pressure resistance of the joint (welded, electrofusion or mechanical).
❓ What is the relationship between this series and ISO 9080?
Answer: ISO 1167 provides the test methods producing raw data; ISO 9080 provides the statistical extrapolation method to long life (e.g. 50 years). Together they underpin the MRS/pressure-rating definitions in pipe standards.
🔒
正在加载下载地址,请稍候 10 秒