BS EN ISO 00899 — Plastics Creep Behaviour Determination Standard Series

Plastics — Determination of Creep Behaviour — Tensile Creep and Flexural Creep by Three-Point Loading (ISO 899 series)

⏳ BS EN ISO 00899 (i.e. BS EN ISO 899) is the British adoption of the European standard EN ISO 899, identical to the ISO 899 series, which specifies methods for determining the creep behaviour of plastics. Creep is the progressive deformation of a material under constant stress over time. It is especially important for plastics — viscoelastic materials that continue to deform under sustained load, potentially affecting the long-term reliability of structural parts, pipes, and seals. The ISO 899 series determines parameters such as creep strain and creep modulus through tensile and flexural creep tests, providing the basis for long-term load-bearing design. The series was prepared by ISO/TC 61 (Plastics) in cooperation with CEN/TC 249 (Plastics).

💡 The “short-term strength” of plastics does not represent long-term load capacity: many plastics continue to deform or even fracture over time under a constant load well below the short-term strength. Creep tests quantify this long-term behaviour.

1. Positioning and Scope 📌

This series applies to the determination of creep behaviour of plastics and plastic products under constant stress (or constant load). Tests are carried out at specified temperature and humidity, applying a constant load and recording the specimen deformation with time, from which creep strain, creep modulus, and creep fracture parameters are calculated. The standard gives specimen dimensions, loading conditions, measurement times, and data-processing methods.

Two parts are included in this batch:

  • BS EN ISO 899-1:2003+A1:2015 — Part 1: Tensile creep, specifying the creep test under tensile loading.
  • BS EN ISO 899-2:2003+A1:2015 — Part 2: Flexural creep by three-point loading, specifying the creep test under three-point bending loading.
⚠️ Part 1 and Part 2 apply to tensile and flexural loading respectively. Real components may be subjected to combined tensile and flexural loading — choose the part matching the actual loading mode.

2. Series Structure and Technical Highlights 📋

StandardCorresponding ISOMain ContentLoading Mode
BS EN ISO 899-1:2003+A1:2015ISO 899-1:2003+Amd.1:2015Tensile creep: constant tensile stress, creep strain and modulusTension
BS EN ISO 899-2:2003+A1:2015ISO 899-2:2003+Amd.1:2015Three-point loading flexural creep: constant bending stress, deflection and modulusBending

2.1 Part 1 — Tensile Creep

BS EN ISO 899-1 specifies creep determination under constant tensile stress. The specimen is subjected to an axial constant load, and the elongation of the gauge length is measured as a function of time, giving the creep strain-time curve, from which the tensile creep modulus is calculated. Amendment A1:2015 updates Annex A.2 (regarding test-condition expression). Tests are usually carried out at specified temperature and humidity; accelerated tests or long-term monitoring may be used where necessary.

2.2 Part 2 — Flexural Creep by Three-Point Loading

BS EN ISO 899-2 specifies creep determination under three-point bending loading. The specimen rests on two supports, a constant load is applied at the centre, and the mid-span deflection is recorded with time, from which the flexural creep strain and flexural creep modulus are calculated. Three-point flexural creep more closely matches the actual loading of beam- and plate-type components. Amendment A1:2015 revises certain content.

💡 Creep modulus is a function of time and temperature: as loading time increases, creep modulus usually decreases (deformation increases). When designing long-term load-bearing components, use the creep modulus corresponding to the time at the design life.

3. Key Technical Requirements 🔧

3.1 Test Conditions

The test should specify and record temperature, humidity, and load level. Temperature and humidity markedly affect creep and should be tightly controlled and stated in the report. The load level should keep the specimen in the elastic or viscoelastic range, avoiding instantaneous overload.

3.2 Load Application and Maintenance

The load should be applied rapidly and smoothly to the set value and held constant, avoiding impact and fluctuation. The instantaneous strain on loading and the subsequent time-dependent creep strain should be recorded separately for analysis.

3.3 Deformation Measurement

A deformation-measuring device of adequate accuracy should be used, recording gauge-length deformation continuously or at set time intervals. Measurement should cover a sufficient duration (from hours to thousands of hours) to reflect long-term creep behaviour.

3.4 Data Processing and Expression

From the deformation data, calculate creep strain, creep modulus (stress divided by creep strain), and give the creep curve. Results should state test conditions, specimen dimensions, load level, and test duration, and where appropriate compare multiple load levels.

🚨 Creep tests are long-duration; temperature and humidity fluctuations introduce noticeable error. Ensure stable environmental control of the test equipment and periodically calibrate the load and deformation measuring systems.

4. Engineering Practice 🛠️

  • 🔍 Long-term design: verify deformation and strength under sustained load using the creep modulus corresponding to the design life.
  • 🔧 Material screening: compare the creep behaviour of different plastics and select materials with adequate creep resistance.
  • 📊 Failure prediction: combine creep fracture data to predict service life under sustained load.
  • 📋 Quality evaluation: use creep performance as an indicator of batch consistency and material stability.

5. Frequently Asked Questions ❓

❓ Q: What is creep?
A: Creep is the progressive deformation of a material over time under constant stress. Plastics are viscoelastic, so creep is significant and must be considered for long-term loading.
❓ Q: How does creep modulus change with time?
A: Creep modulus is defined as stress divided by creep strain. As time increases, creep strain increases and creep modulus usually decreases, indicating reduced stiffness over loading time.
❓ Q: What is the difference between Part 1 and Part 2?
A: Part 1 is tensile creep (axial tension); Part 2 is flexural creep by three-point loading (beam bending). Choose the part matching the actual loading mode of the component.
❓ Q: Why are creep tests long?
A: Creep is a time-dependent process; reflecting long-term behaviour requires sustained duration (hours to thousands of hours). Environmental control and long-term stability are critical to results.
🔒
正在加载下载地址,请稍候 10 秒

Leave a Reply

Your email address will not be published. Required fields are marked *