🔥 BS EN 62739 is the British Standards Institution (BSI) adoption of EN 62739, identical to IEC 62739, covering test methods for erosion of wave soldering equipment using molten lead-free solder alloy. The series is maintained by BSI Technical Committee EPL/501 (Electronic assembly technology & Printed Electronics), classified under ICS 31.190 (Electronic assemblies) and ICS 31.240 (Electronic components). Wave soldering is a common process for soldering through-hole (THT) components on printed circuit boards (PCBs); molten solder erodes/corrodes the metallic parts of the wave soldering equipment (such as the solder pot, rails, pump body and impeller). With the promotion of lead-free solders (e.g. SAC305), the higher soldering temperature and stronger dissolving effect make equipment erosion a prominent issue. The series specifies test methods for evaluating the erosion of wave soldering equipment metal materials in molten lead-free solder, and provides a guide for selecting the appropriate erosion test method.
💡 Lead-free solders (typically Sn-Ag-Cu alloys such as SAC305) have higher melting points and soldering temperatures than traditional lead-tin solder, and erode equipment metals more aggressively; this series quantitatively evaluates the erosion/dissolution rate of materials in molten lead-free solder through standardised tests, providing the basis for equipment material selection and life estimation.
1. Scope and Basic Framework 📌
The series was prepared by IEC TC 91 (Electronics assembly technology) and comprises three parts, all under ICS 31.190 / 31.240. The structure is:
| Standard | Subject | Corresponding IEC | Key Content |
| BS EN 62739-1:2013 | Erosion test method for metal materials without surface processing | IEC 62739-1:2013 | Erosion evaluation of metal materials in molten lead-free solder (no surface processing) |
| BS EN 62739-2:2016 | Erosion test method for metal materials with surface processing | IEC 62739-2:2016 | Erosion evaluation of metal materials in molten lead-free solder (with surface processing) |
| BS EN 62739-3:2017 | Selection guide for erosion test methods | IEC 62739-3:2017 | Guide for selecting erosion test methods for wave soldering equipment |
⚠️ Note: the UK committee voted against the approval of EN 62739-1, considering that current European practice is for suppliers of lead-free wave soldering equipment to perform the relevant tests to demonstrate fitness of purpose. Purchasers referencing the series should therefore require suppliers to provide appropriate fitness-of-purpose evidence.
2. Series Structure and Technical Points 🔧
2.1 Part 1: Metal materials without surface processing
BS EN 62739-1 specifies the test method for evaluating the erosion of metal materials without surface processing (uncoated/unplated) using molten lead-free solder. Typically, a metal specimen of specified dimensions is rotated/immersed in molten lead-free solder for a specified time, and its mass loss or dimensional change is measured to derive the erosion rate, used to compare the molten-solder erosion resistance of different materials.
2.2 Part 2: Metal materials with surface processing
BS EN 62739-2 specifies the erosion test method for metal materials with surface processing (plated/coated). Surface treatments (e.g. nickel, chromium, titanium plating) are often used to improve the erosion resistance of metallic parts of wave soldering equipment; this part evaluates the erosion resistance of the surface layer in molten lead-free solder, assessing the protection of the substrate by the coating and the failure process.
2.3 Part 3: Selection guide for erosion test methods
BS EN 62739-3 provides a guide for selecting erosion test methods for wave soldering equipment, helping users choose between Parts 1 and 2 according to the equipment material, surface-processing state, service conditions and evaluation purpose, and explaining the applicability and limitations of each method.
3. Key Technical Requirements and Test Definitions 🔍
The series centres on the following key technical concepts:
- Erosion: the dissolution and attack of metal materials in molten solder, causing mass loss, dimensional reduction and surface roughening.
- Test conditions: composition and temperature of the molten lead-free solder (e.g. SAC305, with a typical test temperature above the melting point), specimen dimensions, immersion/rotation speed and duration.
- Erosion rate: mass loss or dimensional change per unit time, the quantitative indicator of the material’s erosion resistance.
- Surface-treatment protection: the protective effect of the plating/coating on the substrate, failure time and failure mechanism.
- Fitness of purpose: the supplier must demonstrate that the equipment material meets the service-life requirement under real operating conditions.
✅ The value of the series lies in quantifying and standardising the “erosion resistance of equipment in molten lead-free solder”: through unified test conditions and erosion-rate evaluation, different materials and surface treatments can be compared on a common scale, guiding equipment material selection and life design.
4. Test Methods and Conformity Assessment 🧪
A typical test flow includes:
- Specimen preparation: prepare metal specimens of specified dimensions and surface state per the standard.
- Molten solder preparation: use a lead-free solder of specified composition (e.g. SAC305), heat to the specified test temperature and maintain stability.
- Immersion/rotation test: expose the specimen to the molten solder under specified conditions for the specified duration.
- Mass/dimension measurement: measure specimen mass and dimensions before and after the test, and calculate the erosion rate.
- Result assessment: compare the measured erosion rate with the design requirement or supplier declaration to determine material suitability.
The solder composition, temperature, duration and erosion rate should be recorded and reported per the standard format.
5. Engineering Practice and Application 🛠️
- 🔍 Wave soldering equipment material selection: select materials and surface treatments resistant to molten lead-free solder erosion to extend the life of the solder pot, rails, pump body and other parts.
- 🔧 Equipment maintenance and life estimation: estimate replacement intervals of equipment parts from the erosion rate and schedule preventive maintenance.
- 📊 Lead-free process conversion: when converting from lead-tin to lead-free solder, assess whether existing equipment materials can tolerate the higher temperature and stronger dissolution.
- 📋 Supplier evaluation: require lead-free wave soldering equipment suppliers to provide fitness-of-purpose evidence and erosion-resistance data.
6. Frequently Asked Questions ❓
❓ Q: Why is erosion by lead-free solder more severe?
A: Lead-free solders (e.g. SAC305) have higher melting points and soldering temperatures, and their alloy composition dissolves iron, copper and other metals more aggressively; hence erosion of metal parts of wave soldering equipment is more serious in lead-free processes.
❓ Q: What is the difference between Parts 1 and 2?
A: Part 1 addresses materials without surface processing (bare metal), while Part 2 addresses materials with surface processing (plated/coated). Actual wave soldering equipment parts are mostly surface-processed; select the relevant part according to the surface state of the equipment part.
❓ Q: Is this series a test method or a product requirement?
A: It is mainly a test-method standard giving the methods and conditions for evaluating material erosion in molten lead-free solder; the specific erosion-resistance requirements are set by equipment design, supplier declarations or purchase contracts, with Part 3 providing a method-selection guide.
🔍 Q: How do I judge whether an equipment material is suitable?
A: Measure the erosion rate by the Part 1 or Part 2 test method and compare it with the design life/supplier declaration; also require the supplier to provide fitness-of-purpose evidence as a basis for procurement and acceptance.
❓ Q: Are the tests dangerous?
A: They involve high-temperature molten solder (typically above 260 °C), with burn and fume risks; they must be conducted under controlled conditions by laboratories with protective facilities and operating procedures.