🔧 BS EN 61858 is the British Standard series adopted by BSI from the European Standard EN 61858 (identical to IEC 61858), covering the thermal evaluation of modifications to an established electrical insulation system (EIS). During product development it is often necessary to modify an already-qualified insulation system — for example, to change one insulating material, alter the impregnating varnish, adjust insulation thickness, or change process parameters. This series specifies how, in such cases, to verify with a relatively small number of tests that the modified system retains its original thermal class. It is an important part of the IEC/TC 112 insulation-system evaluation framework.
💡 Unlike a “from-scratch” full evaluation (e.g. BS EN 61857), BS EN 61858 addresses modifications to an already mature system, so it requires fewer tests and a shorter cycle — ideal for material substitution and process optimisation.
1. Series Overview and Scope 📌
The series is developed by IEC/TC 112 (Evaluation and qualification of electrical insulating materials and systems) and coordinated in the UK by Technical Committee GEL/112. This batch of British Standards comprises two parts:
- Part 1: Wire-wound winding EIS (BS EN 61858-1:2014, identical to IEC 61858-1:2014), covering insulation systems of round-wire wound windings and specifying the thermal-evaluation method for modifications to an established EIS.
- Part 2: Form-wound EIS (BS EN 61858-2:2014, identical to IEC 61858-2:2014), covering insulation systems of form-wound (pre-formed) windings and specifying the evaluation method for modifications.
The series concerns thermal evaluation of electrical insulation systems and is classified under ICS 29.080.30. The 2014 edition of Part 1 supersedes the combined BS EN 61858:2008; Part 2 was renumbered from the former BS IEC 61858-2:2014. Both parts were approved by CENELEC on 19 March 2014.
⚠️ The premise of this series is an “established” insulation system — one that has already been qualified and has a defined thermal class. For a first-time evaluation of a brand-new system, use the BS EN 61857 series instead.
2. Series Structure and Technical Points 📊
| Standard | Corresponding IEC | Title | Scope |
| BS EN 61858-1:2014 | IEC 61858-1:2014 | Electrical insulation systems — Thermal evaluation of modifications to an established EIS — Part 1: Wire-wound winding EIS | Thermal evaluation of modifications for round-wire wound winding insulation systems |
| BS EN 61858-2:2014 | IEC 61858-2:2014 | Electrical insulation systems — Thermal evaluation of modifications to an established EIS — Part 2: Form-wound EIS | Thermal evaluation of modifications for form-wound winding insulation systems |
💡 Parts 1 and 2 are divided by winding type: wire-wound windings are typically random round-wire windings, while form-wound windings are pre-formed coils; their structure and evaluation requirements differ.
3. Key Technical Requirements 🔧
3.1 Overall approach to modification evaluation
The standard adopts a “reference-system versus candidate-system” comparison strategy: the original established system serves as the reference system, and the modified system is the candidate system. By comparative testing, the standard determines whether the modification changes the thermal-life behaviour of the system. If the modified system behaves equivalently to, or better than, the original system, the modification is accepted without repeating the full life test.
3.2 Types of modification to be evaluated
- Material substitution: replacement of one or more of the conductor insulation, slot insulation, phase insulation, impregnating varnish or binding material.
- Structural or process changes: changes in insulation thickness, impregnation method, curing process, winding tension, or assembly clearance.
- Supplier or grade change: using materials of similar technical parameters but different origin.
3.3 Test methods and evaluation
The standard specifies the evaluation procedures, including ageing-temperature selection, ageing periods, specimen quantities, diagnostic tests, and acceptance criteria. Diagnostic tests typically cover electrical strength and insulation resistance. By comparing the performance-degradation curves of the reference and candidate systems under the same ageing conditions, the acceptability of the modification is determined. The tests must be statistically representative enough to distinguish genuine performance differences from test scatter.
✅ Key point: the essence of modification evaluation is “equivalence” verification, not re-determining an absolute life value. If the modified system is shown to be thermally no worse than the original, the evaluation passes.
4. Engineering Practice 🛠️
- 🔍 Motor winding material substitution: motor manufacturers use the series to quickly verify that a new varnish or slot-insulation supplier maintains the original thermal class.
- ⚙️ Transformers and reactors: dry-type transformer and reactor coils, after insulation-structure optimisation or process improvements, are evaluated per the series.
- 📋 Supplier change management: when procurement sources or material lots change, modification evaluation controls the stability of the insulation-system quality.
- 📊 Certification and continued conformity: after certification, when insulation changes occur, the series demonstrates that the change does not reduce the insulation class, preserving the validity of the certificate.
5. Frequently Asked Questions ❓
❓ Q: What is the difference between this series and BS EN 61857?
A: BS EN 61857 evaluates a brand-new insulation system (determining temperature index and thermal class); this series evaluates modifications to an established system (verifying equivalence), requiring fewer tests.
❓ Q: What is an “established” insulation system?
A: One that has already been evaluated by an accepted procedure (e.g. BS EN 61857 or the IEC 60505 framework), has a defined thermal class, and has been validated in service.
❓ Q: Does a modification always require a full thermal-ageing test?
A: Not necessarily. Depending on the nature and extent of the change, a comparative or simplified procedure may be used; but the reference system must be the baseline for comparability, and the diagnostic items must reflect the effect of thermal ageing on key performance.
🔍 Q: Why are Parts 1 and 2 separate?
A: Because wire-wound and form-wound windings differ in structure, insulation constituents and failure mechanisms, so separate test models and evaluation requirements are more scientifically sound and accurate.