🔋 BS EN 61056 is the British Standard adopting, identically, the IEC 61056 European standard series for general purpose valve regulated lead-acid batteries, giving general requirements, functional characteristics, test methods, and dimensions, terminals, and marking requirements. Developed by IEC/TC 21 (Secondary cells and batteries), approved by CENELEC as EN 61056, and adopted in the UK by committee PEL/21, it covers “general purpose” (as distinct from fixed stationary-plant applications) valve regulated (maintenance-free) lead-acid batteries for portable, power tool, emergency lighting, fire alarm, and general industrial equipment applications.
💡 BS EN 61056 addresses “general purpose” valve regulated lead-acid batteries; by contrast, BS EN 60896 addresses “stationary” valve regulated lead-acid batteries. Applications, life assessment, and requirement items differ — distinguish by installation purpose when selecting.
1. Scope and General Framework 📌
The BS EN 61056 series applies to general purpose valve regulated lead-acid batteries (VRLA), i.e. lead-acid batteries sealed by means of a safety valve and requiring no topping-up. The series structure is:
- Part 1: General requirements, functional characteristics — Methods of test: general requirements, functional characteristics (capacity, charging, life, etc.), and corresponding test methods for general purpose VRLA batteries.
- Part 2: Dimensions, terminals and marking: external dimensions, terminal types and arrangement, polarity marking, and nameplate requirements.
ICS classification is 29.220.20. BS EN 61056-1:2012 corresponds to IEC 61056-1:2012 (superseding the 2003 edition); BS EN 61056-2:2012 corresponds to IEC 61056-2:2012 (with October 2012 corrigendum, superseding the 2003 edition).
⚠️ Coordination of Part 1 and Part 2: Part 1 defines “performance requirements and how to test”, while Part 2 defines “dimensions, terminal specifications, and marking”. Both are needed for selection, installation, and acceptance.
2. Series Composition and Technical Points 🔧
| Standard | Title | Focus | IEC Equivalent | Status |
| BS EN 61056-1:2012 | General requirements, functional characteristics — Methods of test | Capacity, charging, life, functional characteristics, tests | IEC 61056-1:2012 | Current (supersedes 2003) |
| BS EN 61056-2:2012 | Dimensions, terminals and marking | External dimensions, terminal types, polarity marking | IEC 61056-2:2012 | Current (incl. 2012 corrigendum) |
1. General Requirements and Functional Characteristics (Part 1)
Part 1 specifies general requirements and functional characteristics for general purpose VRLA batteries:
- General requirements: construction, materials, safety valve and sealing requirements, and test conditions.
- Functional characteristics: rated voltage, rated capacity (e.g. C20, C5 discharge rates), charging characteristics (constant voltage/current), self-discharge, and internal resistance.
- Life characteristics: test and assessment of cycle life and float/stand life.
- Test methods: capacity test, charging test, overcharge test, mechanical strength, and sealing tests.
2. Dimensions, Terminals and Marking (Part 2)
Part 2 specifies dimensions, terminals, and marking for general purpose VRLA batteries:
- External dimensions: dimension series and tolerances for length, width, and height (including terminals).
- Terminal types: terminal (post) types, dimensions, and arrangement.
- Polarity marking: marking (colour/symbol) and orientation of positive/negative terminals.
- Nameplate requirements: rated voltage, capacity, model, and other nameplate information.
💡 Standardisation of dimensions and terminals is significant: it ensures batteries of the same specification from different manufacturers are interchangeable in the same battery box/equipment, while polarity marking prevents reverse-connection accidents during installation.
3. Key Technical Requirements 🔬
Key technical requirements for general purpose VRLA batteries include:
- Capacity and discharge rate: rated capacity is defined at a specified discharge rate (e.g. 20-hour rate); capacity varies with discharge rate.
- Charging characteristics: VRLA batteries use voltage-limited constant-voltage charging; overcharge leads to water loss and thermal-runaway risk.
- Sealing and safety valve: the safety valve opens/closes at a set pressure; gas-tightness requirements prevent electrolyte leakage.
- Life: cycle life and float life are key bases for selection and replacement intervals.
- Dimensions and terminals: dimension tolerances, terminal types, and polarity marking ensure interchangeability and installation safety.
🚨 VRLA batteries still require protection from overcharge and high-temperature environments: overcharge decomposes water producing gas, and valve venting leads to irreversible water loss; high temperature accelerates grid corrosion and life decay. Use a matched charger and control ambient temperature.
4. Engineering Practice and Application 🛠️
- 🔍 Selection: determine capacity and discharge rate by load power and discharge time, and verify dimensions (battery box space) and terminal types.
- 🔧 Installation: connect correctly by polarity marking, observe terminal torque and insulation protection, and avoid short-circuit and reverse connection.
- 📊 Use and charging: use a matched charger (appropriate voltage/current) and periodically check voltage and terminal contact.
- 📋 Maintenance and replacement: record charge/discharge and ageing status, and replace promptly per life assessment.
5. Frequently Asked Questions ❓
❓ Q: What do Part 1 and Part 2 govern respectively?
A: Part 1 governs “performance and testing” — the capacity, charging, life, and other functional requirements the battery must meet and how to test them; Part 2 governs “dimensions, terminals, and marking” — external dimensions, terminal types, and polarity marking.
🔋 Q: What does “general purpose” mean?
A: It means general-purpose applications as distinct from fixed (stationary-plant) applications, such as portable, emergency lighting, fire alarm, and general industrial equipment valve regulated lead-acid batteries; the requirement items differ from the stationary series (BS EN 60896).
🔌 Q: Why is terminal polarity marking important?
A: Reverse connection can damage equipment or even cause battery explosion risk. Standardised polarity marking (+/− symbols and colours) and terminal arrangement prevent installation errors and ensure safety.
📊 Q: How is VRLA battery life extended?
A: Use a matched charger and avoid overcharge, control ambient temperature, avoid deep discharge and long over-discharge storage, periodically check voltage and terminals, and maintain per manufacturer recommendations.