🔥 BS EN 60974 is the UK national standard implementing the European standard series EN 60974, identical to IEC 60974 of the International Electrotechnical Commission, prepared by IEC/TC 26 (Electric welding equipment) with UK participation through Technical Committee WEE/6 (Electric arc welding equipment). The series specifies the safety, performance, electromagnetic compatibility (EMC), and test requirements for arc welding equipment (welding power sources, torches, wire feeders, cooling systems, etc.), and is an important technical basis for the design, manufacture, certification, and safe on-site use of arc welding equipment.
Arc welding equipment forms a complete system from power source to torch, wire feeder, and cooler, each subsystem having specific electrical, mechanical, and thermal safety requirements. The EN 60974 series is organised by “whole machine + subsystems”: Part 1 states the general safety requirements (electric shock, heat, mechanical, EMC) and ratings for welding power sources; Parts 2–13 specify, respectively, plasma cutting systems, torches and guns, wire feeders, cooling systems, safety, EMC requirements, ratings and test methods, arc striking and stabilising devices, and test plates. Each part gives the corresponding performance and test criteria.
| Part | Technical Subject | Edition |
|---|---|---|
| Part 1 | Welding power sources — safety requirements and ratings | 2012 |
| Part 2 | Liquid cooling systems | 2013 |
| Part 3 | Power sources for arc welding and plasma cutting | 2014 |
| Part 4 | Current-limiting devices / intershield | 2016 |
| Part 5 | Wire feeders | 2013 |
| Part 6 | Limited-input manual arc welding systems | 2016 |
| Part 7 | Torches and guns | 2013 |
| Part 8 | Gas-shielded metal arc welding equipment (GMAW/MIG-MAG, etc.) | 2009 |
| Part 9 | Installation and EMC guidelines | 2014 (A1:2015) |
| Part 10 | EMC requirements | 2014 (A1:2015) |
| Part 11 | Electrode holders and earth clamps | 2004 |
| Part 12 | Plasma cutting systems | 2011 |
| Part 13 | Welding test plates / trials | 2011 |
This standard is identical to IEC 60974-1:2012 and specifies the general safety requirements for arc welding power sources: protection against electric shock (open-circuit voltage limits, insulation, earthing), protection against heat (overload, temperature rise), mechanical safety, clearances and creepage distances, marking, and instructions, together with ratings (rated welding current, duty cycle, maximum welding current, etc.). It supersedes BS EN 60974-1:2005 and is the core safety specification for the whole machine.
Arc welding equipment is a potential source of electromagnetic disturbance and may also be affected by radio-frequency interference. Part 10 specifies the EMC requirements (emission and immunity limits) for arc welding equipment; Part 9 gives installation and EMC guidance (correct wiring, earthing, distance from sensitive equipment) to help users meet the electromagnetic environment requirements in actual conditions.
Part 5 specifies the electrical and mechanical safety, wire-feeding accuracy, and tests of wire feeders; Part 7 specifies temperature rise, insulation, mechanical strength, and safe use of torches and guns; Part 2 specifies the flow, temperature rise, pressure, and earth-leakage protection of liquid cooling systems. These subsystems together ensure stable and safe welding.
Part 12 specifies the safety and performance of plasma cutting systems (high-voltage arc striking, cutting current, gas paths); Part 11 specifies the current capacity, temperature rise, insulation, and mechanical-strength requirements of electrode holders and earth clamps for manual metal-arc welding.