💡 This article is a scanned-version write-up based on public-domain knowledge. BS EN 60317 is the UK-implemented series of specifications for particular types of winding wires (magnet wires), adopted by BSI from IEC 60317 and maintained by Technical Committee GEL/55 (Winding wires), classified under ICS 29.060.10. This batch contains 51 documents, consisting of 0-x general requirements (e.g. -0-1 enamelled round copper wire, -0-2 enamelled rectangular copper wire, -0-3 enamelled round aluminium wire) and numerous parts for specific insulation combinations and conductor types (−2 through −62). It is the product-specification basis for enamelled and wrapped wires used in motors, transformers, relays and electromagnetic coils.
💡 60317 uses a “general (0-x) + specific wire type (n-x)” structure: the -0-x parts set the general requirements for a conductor class, while numbered parts define specific insulation materials, insulation thickness classes and temperature indices; selection follows the insulation combination to the corresponding part.
1. Overview and Scope 📌
BS EN 60317-0-1:2014 sets the general requirements for enamelled round copper wire, superseding the 2008 edition; -0-2:2014 for enamelled rectangular copper wire; -0-3:2008+A1 for enamelled round aluminium wire. The remaining parts (-2, -3, -8, -13, -20, -23, -27, -35, -46, -51 etc.) give product specifications for specific insulation materials and constructions (polyester, polyurethane, polyimide, glass fibre, aromatic polyamide etc.) and conductors (round/rectangular, copper/aluminium). Earlier editions (1995–1997) are mostly legacy IEC 60317 mappings (e.g. -2, -7, -12, -13, -17, -18), followed by multiple new-edition updates in 2012–2016.
The scope covers conductors for windings of motors, transformers, solenoids and relays, specifying conductor sizes, insulation thickness, temperature index (120, 155, 180, 200, 220 classes), breakdown voltage, pinhole and continuity requirements.
⚠️ The insulation class (temperature index) of the winding wire determines the motor temperature-rise margin. Choosing the wrong class accelerates insulation ageing, causing turn-to-turn faults or burning; conductor type (round/rectangular, gauge) must also satisfy current and slot-fill design.
2. Series Composition and Technical Points 🔧
The table below lists principal parts of the series (based on the real file list in the material, numbering covering 0-1 to 62).
| Standard | Subject | Edition | Remark |
| BS EN 60317-0-1 | General: enamelled round copper | 2014 | Supersedes 2008 |
| BS EN 60317-0-2 | General: enamelled rectangular copper | 2014 | Supersedes 1998 |
| BS EN 60317-0-3 | General: enamelled round aluminium | 2008+A1 | Aluminium general |
| BS EN 60317-0-4/-0-5 … | General: other conductors/structures | 2016/2007 | Rectangular, wrapped etc. |
| BS EN 60317-2 / -7 | Specific types (legacy numbering) | 1996/1995 | Legacy IEC mapping |
| BS EN 60317-8 / -13 | Polyester/polyurethane enamelled | 2010 | Different insulation combos |
| BS EN 60317-20 / -21 | Specific temperature-index wires | 2014 | Heat class |
| BS EN 60317-27 / -28 | Specific insulation wires | 2014 | Insulation-specific |
| BS EN 60317-31 / -32 / -33 | Glass-fibre/wrapped wires | 2016 | High-temperature wrapping |
| BS EN 60317-35 / -36 / -37 | Specific enamelled wires | 2014 | Heat/solvent resistant |
| BS EN 60317-46 / -47 | Aromatic polyamide wrapped | 2014 | High heat resistance |
| BS EN 60317-51 … -62 | Specific wire types | 2016/2012 | Later additions |
The file list shows many early files (1995–2006) retain legacy IEC numbering and exist as scans, while 2012–2016 saw concentrated updates of the -0-x general parts and numerous specific types, reflecting continuous specification evolution. Numbering from -0-1 to -62 covers round/rectangular, copper/aluminium and enamelled/wrapped combinations.
💡 Three selection factors: conductor material and cross-section (current and slot fill), insulation material (heat and solvent resistance) and insulation thickness class (voltage margin). All three must be satisfied simultaneously — none can be omitted.
3. Key Technical Requirements 🔥
Key technical requirements of winding-wire specifications include:
- Conductor size: round diameter or rectangular width/thickness with tolerances, affecting resistance and slot fill.
- Insulation thickness: graded classes (e.g. 1, 2, 3), determining withstand and creepage margin.
- Temperature index: long-term allowable temperature class (120/155/180/200/220), matched to motor thermal design.
- Breakdown voltage: minimum breakdown or withstand voltage, verifying insulation integrity.
- Pinholes and continuity: pinhole count and continuity tests preventing turn-to-turn faults.
- Flexibility and adhesion: film adhesion and cracking under winding, bending and stretching.
- Thermal shock and solvent resistance: insulation must not crack after thermal shock and must resist varnish-impregnation solvents.
🚨 Breakdown voltage and pinhole tests directly reflect insulation quality. Scratches and sharp bends during winding damage the film; smooth guides and proper tension are required to prevent turn-to-turn faults and partial discharge.
4. Engineering Application 🛠️
- 🔍 Selection: based on motor/transformer design (temperature rise, current, slot shape), choose the -0-x general part plus the corresponding specific wire-type part, verifying temperature index and insulation thickness.
- 📋 Incoming inspection: sample conductor size, insulation thickness, breakdown voltage and pinholes to control batch consistency.
- 🔧 Process control: winding tension, turn radius and impregnation must match the insulation class to prevent film damage.
- ♻️ Version updates: -0-x and many parts are updated to 2012–2016 editions; procurement specs should align, since most 1995 editions are superseded.
✅ A “motor temperature rise—temperature index—insulation thickness” matching table embedded with winding process parameter control significantly improves motor life and reliability.
5. Frequently Asked Questions ❓
❓ Are BS EN 60317 and IEC 60317 the same?
Answer: Technically identical; BS EN 60317 is the UK national adoption of IEC 60317, and the BS EN designation governs in the UK market.
❓ What do temperature indices 155, 180 and 220 mean?
Answer: They denote the maximum long-term temperature (°C) the insulation can sustain — e.g. class 155 corresponds to a long-term heat resistance of 155 °C. Motors with higher temperature rise need higher-class winding wires.
❓ How are specific parameters confirmed given the “scan” files?
Answer: Most of the 51 documents are scan-based. This article is based on the machine-readable forewords (-0-1/-0-2/-0-3) and public-domain knowledge of IEC 60317; specific sizes and limits should be taken from the official BSI version.
❓ What is the difference between rectangular and round winding wires?
Answer: Rectangular wire (-0-2) has higher slot fill and better heat dissipation, used in large motors and transformers; round wire (-0-1) is easier to wind, used in smaller windings.