BS EN 50363 — Insulating, Sheathing and Covering Materials for Low-Voltage Energy Cables Standard Series

Insulating, sheathing and covering materials for low-voltage energy cables — the CENELEC cable-compound standard
⚠️ This series includes 11 scanned documents. Content for scanned parts is prepared from publicly available domain knowledge; exact values and clauses must be verified against the official BSI publication.

🔌 BS EN 50363 is the UK version of EN 50363 (Insulating, sheathing and covering materials for low-voltage energy cables), prepared by CENELEC TC 20 and adopted as British Standards by Technical Committee GEL/20/17 (Low voltage cables). The series defines the composition, performance requirements and test methods for insulating, sheathing and covering materials used in low-voltage (≤450/750 V) energy cables. It superseded and consolidated the material information formerly dispersed in HD 21 and HD 22 harmonization documents, and is the core technical basis for material selection in the design, type testing and procurement of low-voltage cables.

💡 EN 50363 is used together with the cable product standards (e.g. BS EN 50525 series): the product standards define the cable as a whole, while EN 50363 defines the technical conditions that the insulating and sheathing compounds must satisfy — the relationship is “product” to “raw material”.

1. Scope and Field of Application 📌

The EN 50363 series is managed by CENELEC with UK participation in Technical Committee GEL/20/17. Part 0 (2011 edition) is the general introduction, replacing the 2005 Part 0; the remaining Parts divide into insulating (Part 1–3 family) and sheathing (Part 4 family) compounds by material type. It applies to elastomeric, thermoplastic and cross-linked polymer compounds used in low-voltage power and control cables, and does not specify the geometry or electrical tests of the finished cable (those are in the product standards).

⚠️ The Parts of EN 50363 should be read together with Part 0, which gives the nomenclature, classification and common test conditions; using a single material Part in isolation may omit general requirements.

2. Series Composition and Technical Scope 🔬

This batch contains 14 documents covering the insulation and sheathing compound sub-families:

PartSubject
BS EN 50363-0-2011General introduction (nomenclature, classification, common test conditions)
BS EN 50363-1-2005PVC insulation compounds
BS EN 50363-2-1-2005 + A1-2011XLPE (cross-linked polyethylene) insulation compounds
BS EN 50363-2-2-2005Thermosetting insulation compounds (EPR etc.)
BS EN 50363-3-2005 + A1-2011PVC sheathing compounds
BS EN 50363-4-1-2005Thermoplastic sheathing compounds (e.g. flexible PVC)
BS EN 50363-4-2-2005Elastomeric sheathing compounds (neoprene etc.)
BS EN 50363-5-2005 + A1-2011Cross-linked polyolefin sheathing compounds
BS EN 50363-6-2005 + A1-2011Elastomeric insulation compounds (EPR type)
BS EN 50363-7-2005Elastomeric insulation compounds (silicone rubber etc.)
BS EN 50363-8-2005 + A1-2011Elastomeric sheathing compounds (CSPE etc.)
BS EN 50363-9-1-2005Thermoplastic elastomer (TPE) insulation compounds
BS EN 50363-10-1-2005TPE sheathing compounds
BS EN 50363-10-2-2005Cross-linked elastomeric sheathing compounds

The series separates into insulation (Parts 1–3, 6–9) and sheathing (Parts 4–5, 8–10) families and further refines by chemical type (PVC, XLPE, EPR, elastomer, TPE), giving each grade its temperature class, mechanical properties and ageing/thermal requirements.

3. Key Technical Requirements 🔥

3.1 General introduction and classification (Part 0)

Part 0 defines the material nomenclature, temperature indices (maximum conductor operating temperature, short-circuit temperature, etc.), common specimen preparation and conditioning, and general test principles. It consolidates the material information previously scattered across HD 21.1, HD 22.1 and similar documents into a single, unified source.

3.2 PVC insulation and sheathing (Parts 1, 3)

Part 1 specifies PVC insulation compounds (e.g. TI1, TI2 temperature grades), checking volume resistivity, heat deformation, thermal ageing, low-temperature performance and mass loss (heat stability). Part 3 specifies PVC sheathing compounds (e.g. TM1, TM2), checking tensile strength, elongation at break, thermal ageing and low-temperature bending.

3.3 XLPE insulation (Part 2-1)

Part 2-1 specifies cross-linked polyethylene insulation compounds, classified by maximum conductor operating temperature (e.g. 90 °C class), checking hot set (heat deformation), mechanical properties before and after ageing, resistance to environmental stress cracking and shrinkage. XLPE is widely used in low- and medium-voltage cables for its excellent heat and electrical performance.

3.4 Elastomer and TPE materials (Parts 4–10)

  • EPR/elastomer insulation (Parts 6–7): EPR and silicone rubber insulation, checking heat resistance, ozone resistance and flexibility.
  • Elastomer sheathing (Parts 4-2, 8): neoprene, chlorosulphonated polyethylene and similar sheaths, checking weather, oil and abrasion resistance and mechanical strength.
  • TPE (Parts 9-1, 10-1, 10-2): thermoplastic elastomer insulation/sheathing and cross-linked elastomer sheathing, balancing flexibility and processability.
🚨 Hot set (heat deformation) is one of the most important quality-control indices for cross-linked materials. Under-cured XLPE or cross-linked polyolefin sheath shows excessive elongation or permanent set in the hot-set test, leading to insulation retraction and local defects under long-term service.

4. Engineering Practice 🛠️

  • 🔍 Cable design and selection: choose the appropriate insulation/sheathing combination from the series by installation environment and temperature class (e.g. PVC for fixed indoor wiring, elastomer for flexible equipment).
  • 🔬 Type testing: cable manufacturers test the insulating and sheathing compounds for mechanical, thermal-ageing and electrical properties per the relevant Part and provide material conformity evidence.
  • 📋 Supply-chain management: incorporate the Part’s indicators into the cable-compound purchase specification to ensure delivered compounds comply with EN 50363.
  • 🔧 Failure analysis: when insulation or sheath fails, re-test the material per the series to locate under-cure, ageing or formulation problems.
💡 Determine the conductor temperature class and environment (indoor/outdoor, oil/weather resistance, flame requirements) first, then match the corresponding temperature-grade Part in EN 50363 — this shortens material selection considerably.

5. Frequently Asked Questions ❓

❓ Q: How do EN 50363 and BS EN 50525 (LV cable product standards) relate?
A: BS EN 50525 defines requirements for the finished cable (construction, voltage, tests); EN 50363 defines the technical conditions for the insulating and sheathing compounds. The two are used together, with the product standard referencing the latter as material-conformity basis.
❓ Q: Why must Part 0 be read together?
A: Part 0 defines the common nomenclature, temperature classes and test conditions on which the specific requirements of each material Part are built; using a Part in isolation may omit conditioning, specimen preparation and other prerequisites.
❓ Q: How reliable are the scanned versions?
A: This series includes scanned files; content has been compiled from public domain knowledge. For specific temperature, elongation and ageing-time values, use the current official BSI publication.
🔍 Q: How is cross-link adequacy of XLPE judged?
A: Perform the hot-set test per the relevant Part: under the specified temperature and load, elongation and permanent set after cooling must stay within limits; exceeding them indicates insufficient cross-linking.
🔒